I wouldnt suggest finishing and blasting in the same area. After time, no matter how clean you are, you will have some cross contamination. Slow down a little and rethink your ideas and don't get ahead of yourself. Finishing with liquid and powder in one booth may be alright, but blasting is not highly recommended.