I done a patch before, and it works best, at least for me, when it is in a "hidden" area, lots of curves etc...To help belnd it in. I did it with black on a quad frame, I sanded the area down real smooth like you would feathering paint in on a car. Taped off the area, but taped it to other "hidden" areas to help hide anything. Then sprayed and cured. Like I said the color was black, so I wet sanded it a bit to get rid of the tape lines, buffed with a clearcoat polish, then it was hardly noticable. Good luck
|