I HAVE FOUND THAT USING A GREEN 10 INCH AIR WAY WITH THE GREEN ROUGE FOLLOWED BY USING WHITE ROUGE ON GREEN AIR WAY WORKS WONDERS BEFORE WHITE ON WHITE.GIVE IT A TRY.I SWEAR BY IT.