Default metal black question

After i clean my bolts up and polish them on a wire wheel, i acid etch them and dip them into blacking solution, soak in distilled water right after, after drying i spray them with clear for protection, finding they are way to glossy. Can i get some opinions here, is there a differant clear coat that does not turn parts glossy looking
Reply With Quote