well, unfortunately my experiences with anodizing have not gone as swimmingly as most others. using caswell's rectifier and LCD i never got a good result, theres a possibility that it has been bad connections all throughout, but before id never had a problem, go figure.
in addition when i did try to run for PAR i never sawi it, just a drop off in current when my volts hit the ceiling
i guess thats why ive been hesitant to completely embrace LCD
|