Default Please define "die casting" metal.

Many motorcycle cases are die cast. I just always mindlessly assumed that die cast "aluminum" was a mix of zinc and aluminum. Two questions, three actually:
1) Is die cast material for structural purposes typically zinc and aluminum or are there other components?
2) What is the typical ratio of zinc to aluminum (for structural castings)?
3) Would you characterize structural diecast material as "pot metal" subject to the known difficulties in plating of pot metal? Or, is it rather more like aluminum (subject to the known difficulties of plating of aluminum by the way)?