Default

duke- beware of coolroom panels--they are disigned to keep low temps not withstand heat so many have insulation that will burn at fairly low temps. If they don't burn they might melt or produce fumes.

Sezer-- Yes many times. Cost is relative to what you have available to you and what you are willing to spend. Time is kinda the same way. The harder you work the faster it gets done.

My current oven took approx 2 days to build and around $800 US.
It will hold 2 motor cycle frames or it has 24 racks that will slide in.9 inside lights and 2 fans with 4 elements. It is stainless steel and aluminum with 2 full length glass doors. Now remember that I have a machine shop at my disposal so materials and equipment are bit different for me.
Here is the best advise for you that I can give(KEEP IT SIMPLE)
Ovens are boxes that heat up, that's all, don't complicate it.