View Single Post
  #13 (permalink)  
Old 07-02-2009, 10:27 PM
SolutionsAutomobile SolutionsAutomobile is offline
Newbie
 
Join Date: Jun 2009
Posts: 44
SolutionsAutomobile is on a distinguished road
Default Re: Which gun to buy

I Agree it does look like a bad ground, but its still a 22 gauge wire thats firmly attached to the bare metal hole. Should I really need a large half inch by half inch square area to properly ground it.

Ive tested my power outlet with a ground fault tool and they ARE grounded. Did that when I was trying to do the same with my chicago gun.

Ive lowered kv to 15-25kv (<1/4)as stated on the gun. Shooting from from 5-8 inches, pressure tried between 5 and 12 psi.

I think Ill try with a OVERKILL ground. Like clip right on bare metal, shooting first coat, then die grinding to bare metal for second coat