I did manipulate the part after first coat. first coat was applied a week ago, Ive touched it with my fingers quite a lot. I do not think it could mess with anything before cure. Sure Id expect weird stuff after cure, like fish eyes, but static should still be attracted to it when shooting it cold. That's just my guess

Could it be that im using too little powder in the hopper? Maybe its not charging the powder enough because of it.

I refused to hot flock, Especially with a gun that shoud easily do 3 coat cold. Hot flocking is messy, and on a thin part like this it cools too quickly. Plus hotflock that pearl and metal flake would make it a paint to get a even consistant looks. Id end up with darker spots and uneven flakes .