Maybe it's just a language barrier, but I'm not sure what you are asking, two posts seem to point to two different things. Are you looking to recover metals after stripping? Please clarify...
Quote:
Originally Posted by almasih86 View Post
actually i am study the composition after dissolved off the plating by using 50% nitric acid and boil it..not from the solution..