Thread
:
Using Masking Agent
View Single Post
#
2
(
permalink
)
12-28-2003, 02:51 PM
mcaswell
Caswell Inc Founder
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries:
1
Yes, use can use Mask-It or any lacquer to prevent areas from plating. Mask-It will peel off after plating. Lacquer would require a lacquer thinner to remove it after plating.