View Single Post
  #9 (permalink)  
Old 07-09-2009, 02:29 AM
almasih86 almasih86 is offline
Newbie
 
Join Date: Jul 2009
Posts: 6
almasih86 is on a distinguished road
Default Re: zinc nickel composition

actually i am working with acid digestion method.im stripped off the zinc nickel plating from metal by using nitric acid and then do 2 titration with EDTA.the first one with murexide indicator then second with xylenol orange indicator.but my problem is the 1st titration which i used murexide indicator is so hard to identify the color change from yellow to reddish violet.now i just put about 3 cristal into it. What is the right amount i should use?