Re: cloudy sections
I've heard you can use diesel fuel or kerosene to clean surface between compounds. Is this true? I think it would be way more cost effective and much less time consuming than hand polishing inbetween different compounds. What is everyones input? Also, if the white, cloudy areas are infact polish buildup, wouldn't hand polishing just contribute to this? Post up guys...
|