I have always used a cheap stainless steel stock pot for dyeing. I've not experienced any problems with it. I have noticed that leaving the dye (Black HBL ) in the pot (nine days old?) exposed to airborne contaminants and evaporation will degrade it in time. I store the dye in airtight plastic jugs.
|