For some reason, im starting to wonder if it isnt more of an LCD issue for me. I had some parts laying around that I did with the old "normal" method and the blue looks alot deeper then it does now using the LCD method. I think that maybe I just notice how much lighter the red is now then I notice with the other colors. Anybody else notice this? Think I should try ano'in at a different current density?