Re: cloudy sections
I guess this is a slow forum? Maybe I stumped some people? Anyway, I did try the kerosene and let me tell you, works way better than any hand polish for the inbetween coumpounds...but to finish a product of I still hand polish when finished cutting/coloring...
|