No problems, potsked. Your answer to my question was exactly what I was expecting.

I'll also agree with potsked on the room temp dyeing. It works quite well, although it might be a bit slower than dyeing with warm dye. However, seeing as how LCD takes about 90 minutes to anodize, another 15 minutes to dye doesn't bother me.