View Single Post
  #4 (permalink)  
Old 01-06-2004, 05:09 PM
tbloss001 tbloss001 is offline
Amateur Metal Finisher
 
Join Date: Apr 2003
Posts: 52
tbloss001
Default

Quote:
Originally Posted by Fireblade
Ahh ok, thanks for the info. I was kind of thinking it was closely related to the actual chroming process itself, just transferring it the other way though. Maybe I shall just continue doing it the way I am now, by blasting it off. I was just curious to this practice, thanks again.
There very well may be a process to do it, that is different/easier than mine if you're already setup to chrome plate. I wouldn't know, as I don't chrome plate things, I usually just remove old chrome so I can gold or silver plate the nickel underneath.

Keep in mind, blasting will certainly remove the old chrome, but it will also remove the old nickel undercoat too. By deplating the old chrome off and keeping the old nickel underneath, you might save yourself a few steps down the road.

Just a thought.
Reply With Quote