I really dont want to change the ano bath mixture yet to go back to teh old method. One thing I hated with the old method is that I wasnt real sure how long to let the parts in. With the new method, it sounds like the connection to the part is a very large concern, which may run me into problems down the road. I just cant tap holes into alot of the parts that I will eventually be doing so that they have a super tight connection! Anyhow, anybody have advise as far as the LCD anodizing is concerned? Thanks!