How to load my wheels properly
I am just starting out with learning how to polish. I am curious of the proper way to load my wheels.
1. Do I need to warm up the compounds?
2. Do I wet the wheels first? if so do I let the compound dry after applying it?
3. Do apply alot of pressure or very little?
I am really unsure of the "Proper" way to load.
|