Not required, but why not. I had done some parts under the hood on my personal truck. Some left uncleared and some i did.They both looked great but you could tell that the cleared parts kept a better shine. And when I had a radiator hose blow, it messed up the finish on the uncleared parts while the others cleaned up pretty good.
|