Default Re: cloudy sections

Have you folks tried using Flitz to remove the cloudiness? Compound residue seems to be the likely culprit, especially if kerosene removes it.

Remember to apply very small amounts of compound to the wheel at a time.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote