Default Re: Look of Chrome Powder Coat?

Not very similar. It looks more like a chrome colored paint...which is really all it is.

There are some yellow pics in our Restoration Forum. No one has sent us any chrome pictures yet.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote