Default Acid Bath Content?

I am having trouble getting certain parts to anodize, some will work but others won't. The acid bath is 10% sulphuric acid with 30g of Sodium sulphate per litre of sulphuric/water solution. I read this off a webpage of a guy who does anodizing with good results, but I have yet to see this mix mentioned since! Does anyone know the reason for the sodium sulphate and could it be causing my problems? I have tried using a 12V charger and also 2 car batteries(ie. to give 24V)the batteries make short work of burning the parts!
Should I make a new acid mix(with just sulphuric acid) and try it with the charger again? I am going to get a light dimmer tomorrow and try keeping a constant current, but I am still limited to 12V.
Any help would be great.
Thanks