Default Copper over nickel problems

I am using a plug and plate system, and am having strange problems. I have followed the instructions with no deviation, and am trying to use a copper plate over nickel to fill minor scratches etc. However, every single time I lay the copper plate on, it bubbles on the nickel and won't bond properly. Any suggestions?