Re: negleted semi wheels
Why don't you try greaseless compounds. They literaly rip the first layer of aluminum off quicker than you can say "concrete slurry". I polish sportbike frames, and I use the 120 grit greaseless on an 8" spiral sewn cotton wheel. works fast and easy. I have a set of rims in my garage right now and they need to be polished but i will need to buy a faster drill and 4" wheels to get in there. PAIN IN THE BUTT!
|