I haven't used Zoop but I hear good things about it.

I, like customandsound, use a high quality carnuba wax on my polished surfaces.

I've tried the VHT clear on polished steel and frankly, I'm not impressed. In my experience, it dulls the finish and it definitely discolors when you cure it according to the can's directions.

A clear poly like is used on automotive finishes might work, but I haven't tried it. (yet)

Another option some folks have used is a clear powder coat. You might want to check out the powder coating forum for more info.