Some old Ford bolts (chassis, wheels, ?etc.) have a dull medium-dark gray finish; parts of these had rusted. After bead plasting some pits remain, although the bolt is now light gray bead-dull. What is the finish to restore? Will it prevent further rust? If rust remains in the tiny pits what is risk of failure? What kit to use?