View Single Post
  #3 (permalink)  
Old 02-11-2004, 10:50 PM
customandsound
Guest
 
Posts: n/a
Default

that is funny this .. that this post was listed ... i got covers from a full dresser i am doing .. and i can't get them to shine .. i wet sanded 40-600 hit with black on a sisal then brown on a spiral then to white on losse cotton... i got a black chrome look going on ... but if you look at an angle it is perfect .. but head on it looks bad ... i was going to bead blast it then start over ...the primary has a nasty mark on the lower half where the controls are .. it looks polished from the factory but i am not sure .. it may be chromed .. if i can't get it i am going to dip it .. and be done with it ..