maybe contaminated wheels? My loose cotton wheels seem to get really dirty and leave black, greasy deposits on parts. I have to rake them quite often to get 'em to color without leaving a mess behind.
I also get 15-20 mins out of an application of greaseless. The 1st couple minutes it cuts like crazy, then seems to lose some "bite", but still removes material, just bit more slowly.
|