i've tried brake clean,carb clean and never dull,the brake and carb clean
will have you feeling nice(not good)and leave a dull haze on aluminum.the never dull was just a newbie mistake.acetone is the way to go,it leaves the metal clean and smooth wich allows you to see spots that might need to be re-buffed and costs about $4.00 a bottle and can be found at just about any automotive parts store.hope this helped.
|