View Single Post
  #5 (permalink)  
Old 02-18-2004, 09:54 AM
bigfishon1 bigfishon1 is offline
Newbie
 
Join Date: Feb 2004
Posts: 6
bigfishon1
Default

Thanks for the feedback! I have heard of the oven cleaner but also heard mixed results. It won't hurt to try. If not I will go with Caswell's stripper. Although if the same as aviation stripper then the wheel will just laugh at it.

Hmmmm...I tried emery on sisal and it also didn't do much.

These wheels are Porsche wheels which are about 30 years old. Not sure if the final finish has been clear coated or clear powder coated. I just know 220 struggles with it and 220 takes a while. And emery doesn't do much.

I will try the suggestions and post.

Thanks!
Reply With Quote