Default Nitric Acid/Desmut problem....Help

I'm running into a problem with a chemical purchased from Hobby Plating.......imagine that. I originally bought desmut from them, before I got the rest of my order as well as the dilution and usage instructions, they had him in jail. At any rate, the 2 five gallon containers I have are marked as follows:

Desmut Concentrate-

Corrosive liquids, Acidic, Inorganic N.O.S. , Nitric Acid Mixture UN-2031 PG ll

Warnings are as follows: Health 3, Flammability0, Reactivity 1, Personal Protection CR

There are a few other warnings on the containers pertaining to emergency treatments and such. Problem being, I didn't get any directions for the dilution or usage of this product. Secondly I wasn't aware of desmut containing nitric acid ( I thought bright dip was nitric acid.) Note... this is not the desmut light product also sold by the aforementioned Rat &@$^@%! at hobby plating. This is the industrial version, probably purchased from another manufacturer with his label stuck on the corner of the manufacturer's contents sticker. The product came in two white, handled, round, 5 gallon, chemical containers. I could sure use some help with this. Lance Caswell advised me to put it out on the forum to see if anybody has dealt with this product. I appreciate the help.
Thanks,
EasTTex
Reply With Quote