View Single Post
  #2 (permalink)  
Old 02-19-2004, 10:59 AM
NeoMoses NeoMoses is offline
Amateur Metal Finisher
 
Join Date: Mar 2003
Posts: 162
NeoMoses
Send a message via AIM to NeoMoses Send a message via Yahoo to NeoMoses
Default

The general information I've found says to use Nitric acid at a 30% (by volume) concentration to desmut. However, most agree that plain nitric acid is not enough to completely desmut, thus there are many proprietary mixtures available.

The main problem I see is this: if you don't know the concentration of the acid you have, how will you know how much to dilute it? Wish I could help you more, but that's about all I know. Perhaps you could contact the manufacturer of the acid if their information is still on the box.
Reply With Quote