Re: Plug n plate kit for bathroom faucets ?
Chrome plate starts to blue around 900°F. Chrome plate should never peel off.
Hard Chrome has very different properties than decorative chrome. It is only used to build very wear resistant surfaces, such as hydraulic cylinders and can also be used to rebuild worn shafts. It is used mainly in an industrial setting and is not a "harder version of decorative chrome."
Hard Chrome is a very dull colored plate.
If plating any part on a bike, you'd use decorative chrome.
Hard Chrome and Decorative Chrome are addressed in the manual, starting on page 89.
|