stryder you are right .. the older bikes the parts were chromed ... i got panhead and a knuckle head sitting in the garage.. that are old as the dirt on them ... for the pitted chromed parts .. get them smooth fill them with lab metal /pyro metal .. dip them with copy chrome or triple dip them