you want to go strictly Corona unless you are specifically coating only epoxy and only have no humidity. Only then will it prevail in helping you coat better. I stongly suggest if you are "upgrading" to get a fluidized bed set-up only for the fact that the little cup on top of the industrial models really has no growth potential involved. The cup is what it as, as to where fluid beds come in all shapes/sizes. Heck... you can even make a fluidized bed or find one at an auction cheaply enough if you so chose. Good luck in expanding your horizons.... Russ