first you must Zincate the part then you can either go to nickle then chrome....or nickle strike(or flash copper), acid copper, nickle then chrome. If you get poor results, try Zincate, then strip in a pickle solution, zincate again then proceed as described above, this ensures you get a good zincate coating proir to nickle.