Default Clearcoat is cracking.....

I coated a cast iron steering steering knuckle with satin clear...It looks like the clear has many spider cracks in it....what is the most likely cause of this? I baked it for about 15 min after flowout at 350 degrees. Then let it cool in oven with heat off. I suspect I either coated too thick, or have an incomplete cure. Whatdoya think?