Okay to you guys that use this stuff... what am I doing wrong?
I load up a pair of Sisal wheels, let it dry... even for a couple of hours one time. Turn it on, hit a part and *!* gone.... I get about 15 seconds of work out of it.
The sisal seems to load on the "threads" sticking out, not the wheel face.
Any tips?
|