Default Flow out and part temperature

I vary my cure time depending on part size....on a large piece like a manifold or bellhousing, I'll start timing the cure once the powder flows out(melts)...

Is powder flow out a reliable indication the part has reached the cure temp? or will flow out occur at a lower temp?

Guess I need to monitor the actual part temperature....and not rely on the old stoves thermostat.