I went out and bought a buffer stand last weekend and will be heading out side. I keep my bike and computer in the garage and don't want it looking like a horse barn. I wonder if Sisal makes good mulch.LOL
Now that I raked the Sisal, and evened it out, it feels a lot smoother. Not so chattery when I apply pressure. I know what you mean though about bracing your self and leaning in to the wheel. that also helps a lot.
Getting pretty good results so far. I can read a news paper in the shine in the aluminum. I stull have "micro fine" buffer marks that show up when the light hits it at the right angle though. That's after I've used White and a loose wheel. I tried rubbing it with baking flower and it cleans up the shine, but doesn't do anything for the micro fine scratches.
Any ideas?
Do I need to polish it by hand now with something like Winol metal polish to remove them?