I would think one of those 2 gallon pancake tank compressors would have more than enough capacity for PCing. With our low pressure requirements, you could even use a 5-6 gallon portable air tank (without a compressor) and a regulator to do the job. Fill it up at the local gas station and go to work PCing. The portable tanks are usually $20-$30 at WalMart, and the pancake compressors are in the $100 range at Home Depot. Maybe even less at someplace like Harbor Freight. At 10-15 psi, you have lots of choices!