I have just recently started using 2" nylon discs for surface prep before plating. I have used medium and fine discs. I think they work really well because they are more gentle on the base metal than sanding discs. I have a tendancy to make more gouges than remove them when using sanding discs. The nylon are good for getting casting lines, pits and gouges out quickly.