View Single Post
  #3 (permalink)  
Old 03-14-2004, 08:58 AM
hybred hybred is offline
Newbie
 
Join Date: Mar 2004
Posts: 29
hybred
Default

yes, the part i am doing next is alum. and i would pre-heat it first. but was wondering if when pre-heating the part it would screw up the polish finnish when the contaminents are realeased as the pores open? maybe i just need to spay it with clear instead? seems alot easier?