What happens when you strip the parts and re-anodize them without bead blasting again? Do they turn out as expected?

I, too, have seen this problem of poor dye absorbtion with colors. Although I haven't determined a root cause, stripping and re-anodizing the parts usually fixes it for me. It's not a good solution, but it is a solution. See if it works for you.