Your power supply is right in no-mans land. Too big to plate the very small stuff (no control in the low amps range) and not enough to do large chrome plating. A 4.5 gal chrome kit will plate 100-200 sq" - no problem, so your unit is actually underpowered for even that kit when it comes to chrome.
Still, you could supplement it by using one of our new 3 amp digital power supplies ( a snip @ $95) and then use the nichrome wire principal for stuff over 50 sq"
Don't think the nichrome wire principal is tacky, it might look it, but its VERY effective- and costs $10!!!!!!!!
I doubt you'd have too much good luck with the wheels idea! But then, our customers are pretty ingenious!!!!
|