Default First Time Anodizing

This is my first time anodizing aluminum. I've never plated or anodized anything before. I bought the anodizing dye and the complete plating manual. The first part that I anodized was a success. I was really impressed with the results. Caswell has a great product.
Rich Bereswill
3:16 Racing