Default Re: Do I really have to use copper over a nickel strike coat

Thanks for the nice comments.

Applying copper might help with the pitting, but more likely it's an agitation problem.

We have heard of that method of agitation and are planning to include it in the next version of the manual.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote