One of you knows how powerful is the light produced by this additive? Is it week or you can really see something in the dark with this stuff. Is the coat uniform or is it full of spots? How is the finish, flat or gloss?
I already use powder like this but I just put it in urethane lacquer. Powder coating it would be very interesting but I need a minimum of light from the part.
sam
|